HIGH SULFUR CP COKE (ANODE GRADE)

TECHNICAL DATASHEET

           
Sr.No. PARAMETERS UOM TYPICAL VALUE

 

GUARANTEED
VALUE
TEST
METHOD
1 Sulphur as S % 2.5 – 3.5 2.5 – 3.5 ISO 12980/ ASTM D6376
or ISO 5931
2 Vanadium Ppm 300 Max 300 Max ISO 12980/
ASTM D6376
ISO8658/
ASTM D5600
3 Nickel Ppm 250 Max 250 Max
4 Calcium Ppm 150 Max 150 Max
5 Iron Ppm 350 Max 350 Max
6 Silicon Ppm 350 Max 350 Max
7 Titanium (Ti) Ppm 15 Max 15 Max
8 Sodium Ppm 100 Max 100 Max ISO 12980/ASTM D6376
or ASTM D5600
9 Ash % 0.35 Max 0.35 Max ISO 8005/ASTM D4422
10 Moisture % 0.30 Max 0.30 Max ISO 11412/ASTM D4931
11 Volatile Matter % 0.50 Max 0.50 Max ISO 9406/ASTM D3175
12 Real Density gm/cm3 2.06 – 2.08 2.06 Min ASTM D2638/ISO 8005
13 Vibrated Bulk Density ASTM
(-20/+48 Mesh)
gm /cm3 0.85 Min 0.85 Min ASTM D4292
14 Electrical Resistivity µΩm 500 Max 500 Max ISO 10143
15 Sizing(%) +25 mm 0% 0% ISO 2325
+4.75mm 25% Min 25% Min
– 0.85 mm 25 % Max 25 % Max
(-) 200 mesh 3% Max 3% Max
16 Phosphorous Ppm 10 Max 10 Max XRF Method

 